Skip to main content

Re: [MW:23739] Impact Test Requirement for Welds of API-650 Storage Tank when Design Metal Temperature is below -7°C

Design code to be followed for impact test requirements. Follow API 650.

On 17 Oct 2015 13:27, "SA" <sarfrazengineer@gmail.com> wrote:
Dear All,

A Fuel Oil tank has been designed as per API-650 code and it is mentioned in this code that when design metal temperature is below -7°C impact test shall be carried out for all welds for all components. The statement in code is given as: 

"9.2.2.2 When the design metal temperature is below -7°C (20 OF), impact tests of the weld metal shall be made for all procedures used for welding the components listed in 4 2.10 1, for welding attachments to these components, and for fabricating shell nozzles and manholes from pipe and forgings listed in 4.5. 

In our case, design metal temperature is below -7°C i.e. -10°C but still welding engineer is insisting that impact testing is not required as per ASME Section IX (QW-403.5).

My question is that Tank is designed as per API-650 and there is no reference that ASME section IX would supersede  the above statement of API-650 where impact testing shall be carried out when Design Metal Temperature is below -7°C.

Can anybody guide on this subject.

Thanks in advance

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b751b08a-e0c5-4b0d-8b76-34555fc91bcd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1%2BN-WtZEryA90%2BS1nV%3DrJB73FkSP0yfXJTtM86go33ZUQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .