Re: [MW:22678] Copper alloy electrodes

Dear Yogesh Pawar,


Kindly see the attached details of options available, to weld MONEL (Cu-Ni)

These are the products of Special Metals-USA.

Also, enclosed is 'Selector Chart' for  Nickel- based Alloys.

In case, you need welding consumables for other Copper-based alloys, then

AMPCO - USA products are available.

Best Regards

Ashok Rai 

On Sat, Dec 27, 2014 at 12:29 PM, 'c sridhar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
 
Nearest available electrode could be monel type with 70 Cu - 30 Ni.

GMAW followed by SMAW is suitable GTAW.

ECuNi- Coated Electrode
Copper-nickel alloys and selected bronzes to themselves and to Alloy
400 or Alloy 200
Electrodes of the Copper-nickel classification are used for shielded metal
arc welding or wrought or cast 70/30, 80/20 and 90/10 copper-nickel alloys
to themselves or to each other. They also are used for welding the clad side
of copper-nickel clad steel. Preheating is generally not necessary.
 
ERCuNi - Filler wire.
Copper-nickel alloys and selected bronzes to themselves and to Alloy
400 or Alloy 200.
In Copper-nickel filler metals, the nickel addition strengthens the weld metal
and improves the corrosion resistance, particularly against salt water. The weld
metal has good hot and cold ductility. Copper-nickel filler metals are used for
welding most copper-nickel alloys. When using the GTAW or GMAW processes,
preheating is not required. Welding is done in all positions

Sridhar.

 


From: Yogesh Pawar <yogeshpawar5@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 25 December 2014 12:19 AM
Subject: [MW:22633] Copper alloy electrodes


Dear all,

Please advice Electrodes details for Copper alloy Materails
Material SB171 C70600 (90Cu-10Ni)
P.No.34 to P.No.34
Thk-40mm
Which welding process is better SMAW or GTAW

Thanks & Regards
Yogesh P.
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJkv1Vo-OJA-wUn9JtkcLYvbjVgyj1b%2BK2PM9woOYnOzcZmZWg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...