Re: [MW:22753] Combining PQR to make new PQR - Help in understanding the concept

Your base metal thickness range is 5 - 40 mm..the deposited fillet metal thickness is 0 -30 mm for GTAW and 0-40 mm for SMAW

Sent from my BlackBerry 10 smartphone.
From: Suhel
Sent: Κυριακή, 25 Ιανουαρίου 2015 - 06:12
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:22752] Combining PQR to make new PQR - Help in understanding the concept

Hello Dear Members,

I have learnt about combining various PQR today in a basics of welding class. I was refering to ASME Section IX to check my understanding, I have a bit of confusion and your help would be appreciated. 

(all the scenarios are imaginary as I just want to understand the concept)


1. PQR1 - 15mm welded completely with GTAW
2. PQR2 - 20mm welded completed with SMAW 

According to the table QW-451.1

PQR 1 will be qualified for - 5mm to 30mm  GTAW &
PQR 2 will be qualified for - 5mm to 40mm  SMAW

So can I have qualified PQR of base metal thickness of 70 mm (30mm GTAW + 40mm SMAW)? If not, then what is the maximum basemetal thickness I can weld combining these two PQRs?


Thanks,
Suhel.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b42f9b0d-e6e2-40e7-851a-59e2491fb4e6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...