Re: [MW:22767] can we prepare new PQR with ASME and AWS and EN standard?...

EN 15614 is more stringent followed by ASME and AWS in order.  

Type and no. tests depend up on material thickness and other 
variable parameters.

Towards AWS, you can  use ASME  PQR as a pre approved document also.

But, U could be more specific .

C Sridhar.

Technical Adviser - Welding,
for Alsta Pristine Engineering Private Limited,. Bangalore

( SS, AL fabricators & A venture of Advance Eng. Training & Inspection Services). Chennai,

Mobile nos: 0 94449 71097, 0 7406 326326, 0 94445 21267.


Please don't print this e-mail unless you really need to. Save the environment.




 


From: Umar Rashid Makrani <firoz.makrani@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, 26 January 2015 10:49 PM
Subject: Re: [MW:22762] can we prepare new PQR with ASME and AWS and EN standard?...

Dear Abdul Ghani,
Make a list of all essential variables, testing requirements and acceptance criteria, check whether single testing can be done? if not you may have to create multiple samples (make sure you weld a coupon big enough). now weld the coupon as per required size and test according to multiple code/standard requirements and prepare multiple Records. Good Luck.
Please update the forum about the results.
Expect the experts to comments.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,
NACE CIP-2, LEEA Registered Engineer.

On Mon, Jan 26, 2015 at 4:57 PM, Mohammed Ghani <ghani386@gmail.com> wrote:
Dear sir,

I have to prepare a single PQR using ASME, AWS and EN 15614. can we prepare such PQR ?
if yes, please let me know which are the main points need to considered. like (thickness, P Number, Group Number, Impact testing). which code is more stringent?

also if possible, refer a code. 
Kindly do needful.

Thanks and regards,
Mohammed Ghani.

On Mon, Jan 26, 2015 at 4:50 PM, <george.dilintas@gr.bureauveritas.com> wrote:
please be more specific

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for ghanicwi---26/01/2015 14:25:59---Dear experts, can we prepare as PQR based on ASME, AWS, and EN standghanicwi---26/01/2015 14:25:59---Dear experts, can we prepare as PQR based on ASME, AWS, and EN standards?

From: ghanicwi@gmail.com
To: materials-welding@googlegroups.com
Date: 26/01/2015 14:25
Subject: [MW:22758] can we prepare new PQR with ASME and AWS and EN standard?...
Sent by: materials-welding@googlegroups.com




Dear experts,

can we prepare as PQR based on ASME, AWS, and EN standards?
If yes, then which are the qualifications (limits) and test are differs with respect to ASME standards,

Kindly do needful.

Mohammed Ghani
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/aa3f596a-d24d-4b0b-afef-3a90f5a67e93%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFDDF5C395.1D8EBCE1-ONC2257DD9.004BF9CD-C2257DD9.004C0135%40LocalDomain.

For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.
 "Be the change you wish to see in the world"
---Mahatma Gandhi---
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVgs55oievajxW%3D%2BaUmUciCv%2B-cmKy%2BJF-wtOFSNjWmyWw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKyjn48Yq5jSqjBybfEUbdzZuAfaX%2B%3DCQ3RR4hUAz1CmxFg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...