Re: [MW:16012] Plate qualifications for piping and process restrictions in ASME

Please specify your code of construction, in general plate qualifications can be used for piping with few exceptions. however for performance qualifications diameter restriction (e.g. >24" dia in ASME BPV IX) are applicable as per the code of construction. Process restrictions will not be specified in ASME, you can refer to API RP 582 or the applicable contract documents

Note: Please post with an appropriate subject line and don't send to individual mail ID's

On Thu, Nov 22, 2012 at 7:39 PM, cyriac dominic <cyriacd@gmail.com> wrote:
Dear Experts,
I am a member of this form and the questions and answers are very much interesting. Now I have got some questions regarding welding.
We have to fabricate some equipments and pipe lines for a geothermal power plant in Africa. The material of the pipe is A106 gr B and material for the equipments is  P265GH which is equivalent to ASTM 516  gr 60. Following are my questions.
1)  Whether we can use the procedure qualifications  which are  done on the plate to qualify the pipe welding ( both are the same P nos)
 2)whether we can use the procedure qualification which is done on the plate  can be used for the performance qualification of welders for pipes?
 3)Our client is not allowing us to weld with GMAW on pressure retaining equipments or components  and instituting  not to use FCAW
  on pressure vessels and piping other than carbon steel. What is the technical reason for that? Or is it some where in the ASME code?..
Please give me some light on that.
Regards Cyriac Dominic

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...