Re: [MW:15963] RE: 15948] Consumable insert for pipe to pipe wlding

these combination of welding not acceptable due to heat treatment
requirement for P91
Pandithan/9940739349
Welding consultant
madurai

On 11/19/12, John Henning <jhenning@deltak.com> wrote:
> You should not be welding P91 to A106.
>
> John A. Henning
> Welding & Materials
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Sankaran Sp
> Sent: Saturday, November 17, 2012 1:38 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:15948] Consumable insert for pipe to pipe wlding
>
> Dear experts,
>
> We are the leading industrial valve manufacturer in Coimbatore ( INDIA),
> we have requirement of pipe to pipe "butt joint" welding by TIG process
> with RT quality.
> Pipe materials are ASTM A 335-P91 & A106 Gr B pipe and sizes are
> 1/2",3/4"& 1"sch 160.
> While welding of pipes we need to maintain 2.0 mm root gap with full
> penetration.
> How to carry out this type of welding with RT quality ?
> Can you give solution for this requirement?
> Can we use consumable inserts between pipes ? If yes where should get
> the consumable inserts in INDIA ? who are the suppliers?
>
> Kindly send your recommendations & address.
>
> Advance thanks and regards,
> Sankaran.SP
> Coimbatore
> INDIA
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&
> trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
>
> ______________________________________________________________________
> The information in this email is confidential, and is intended solely for
> the addressee(s). If you are not the intended recipient of this email please
> let us know by reply and then delete it from your system; you should not
> copy this message or disclose its contents to anyone. The internet can not
> guarantee the integrity of this message. HAMON (and its subsidiaries) shall
> (will) not therefore be liable for the message if modified.
> ______________________________________________________________________
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...