Dear Experts
I have little query about qualifying the WPS as per AWS D1.1-2008 (Chapter 3 Prequalification of WPSs)
Actually I need to qualify a WPS on IS 2062 material, but material is not mention in the table 3.1 and as per clause 3.3 only base metals and filler metals listed in Table 3.1
may be used in prequalified WPSs.
so kindly guide me how to make prequalified WPS else I Have to qualify the procedure with testing (Chapter 4).
Waiting for your quick response.
With Regards
Rakesh Kumar Bilara
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.