Tuesday, November 15, 2011

[MW:12981] Joint preparation-root gap

Dear All,


I have problem in joint preparation. According to design drawing & WPS the root gap for welding 48mm carbon steel plate by SMAW process is 3 mm, but actual we have gap more than 10 mm. This welding is for pressure vessel (ASME VIII Div.2). 
Can we weld this joint with gap more than 10 mm? as per ASME IX for SMAW process root gap is not essential variable. Thanks

Best regard,


Lukman

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...