Skip to main content

Re: [MW:9026] RE: 9018] Stress Corrosion Cracking Test

Hi Elumali,

Thanks for quick feedback.

Yes, it is corrosion test and being done at laboratory having appropriate set up. But the question is that project specification requires it as per ASTM  G 36 ,with cacl2 solution.

Request to provide more information, if available.
regards,
jignesh rana


----- Original Message -----
From: Sundaram Elumalai
To: materials-welding@googlegroups.com
Sent: Thu, 30 Dec 2010 17:06:10 +0530 (IST)
Subject: [MW:9021] RE: 9018] Stress Corrosion Cracking Test


















Hi,



 



This is one corrosion test need to be done
at approved Lab. So you may check in your region, who is doing this test.



 





With Kind regards,



 



S.Elumalai.














From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jignesh.rana@Linde-LE.com

Sent: Thursday, December 30, 2010
1:45 PM

To: 'materials-welding@googlegroups.com'

Subject: [MW:9018] Stress
Corrosion Cracking Test





 





Dear Members,



One
of our project specification calls for Chloride Stress Corrosion Cracking as
the ASTM G 36 with CaCl2 (40%) solution for super Duplex Stainless steel ( S
32750)




ASTM
G- 36 is based on MgCl2 solution.




Does
any one having experience with SCCT with CaCl2 solution ?




With
Best Regards,



Jignesh R Rana

Manager - QA & QC



Linde Engineering India Pvt. Ltd.

38, Nutan Bharat Society, Alkapuri, Vadodara 390007, India

Tel.: +91 265 3056789, Fax: +91 265 2335213 , Mobil:  +91 90999 86019

jignesh.rana@linde-le.com, www.linde-india.com



This e-mail is confidential. If you are not the intended recipient, please
notify us immediately. You should not disclose its contents to any other person
nor use it for any purposes.





--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.











--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...