Skip to main content

Re: [MW:8926] Problem of PWHT

On a mechanical CS line after a 0.75" valve instrumentation impulse
line is coming which is of P11 material...........welding done using
ER70S-B2L. .....and now can I do PWHT to that joint which is to b done
as per procedure of alloy steel...since this joint is between AS to CS
is there any problem in doing PWHT

On 12/24/10, Yogesh kumar <yogeshandpini@gmail.com> wrote:
> Hi vivek
>
> Will you please elaborate more your CS/AS joint configuration is not
> getting clear to me??
> yogesh.
>
>
> On Fri, Dec 24, 2010 at 9:25 AM, vivek m <vivekmohan007@gmail.com> wrote:
>
>> The impulse line is of P11 material and it has to be post heated...i
>> want to knw d problems dat may occur to the 0.75 joint between cs and
>> as
>>
>> On 12/23/10, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
>> wrote:
>> > Generally Impulse lines are outside scope of ASME B31.3 and don't
>> > require
>> > PWHT. Even if it is designed by B31.3 it doesn't require PWHT as
>> thicknesses
>> > low, , unless it is a contractual requirement
>> >
>> > -----Original Message-----
>> > From: materials-welding@googlegroups.com
>> > [mailto:materials-welding@googlegroups.com] On Behalf Of vivek m
>> > Sent: Thursday, December 23, 2010 9:34 PM
>> > To: materials-welding@googlegroups.com
>> > Subject: [MW:8914] Problem of PWHT
>> >
>> > Dear all,
>> > one of my P11 impulse pipe (0.75") is connected to a CS 0.75" valve
>> > which comes with big bore CS line (all as per drawing)......now shall
>> > i do pwht to that joint ? If done will there be any problem to that
>> > joint ...please give me a detailed answer.
>> >
>> >
>> > Filtered by Hosted Filtering
>> >
>> >
>> > --
>> > To post to this group, send email to materials-welding@googlegroups.com
>> > To unsubscribe from this group, send email to
>> > materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscribe@googlegroups.com>
>> > For more options, visit this group's bolg at
>> > http://materials-welding.blogspot.com/
>> > The views expressed/exchnaged in this group are members personel views
>> and
>> > meant for educational purposes only, Users must take their own decisions
>> > w.r.t. applicable code/standard/contract documents.
>> >
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscribe@googlegroups.com>
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...