Hi,
 
AWS D1.1 does not restrict weld metal deposit. It restrict base metal thickness.

Regards,
Ibrahim
On 5 April 2010 17:53, Shashank Vagal <nach_sam@yahoo.com> wrote:
Hi all,
We qualified some welders to 6GR on  6" dia x 7 mm thick pipes using SMAW  for root + hp (deposited about 4 mm) followed by FCAW. Now, if we want to use these welders for full SMAW - i) Is it allowed? ii) What is the new qualification to?
S Vagal


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...