RE: [MW:29133] derivation welds

Dear Sr.

 

Comment  that there aren´t owner specs. We just support in design code regulations.

 

So, about your information, could you have some code/standard reference to review in detail?

 

Thanks in advance.

 

Best Regards

 

Miroslav Tadic

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de muneebslsa@gmail.com
Enviado el: martes, 19 de febrero de 2019 02:04
Para: materials-welding <materials-welding@googlegroups.com>
Asunto: Re: [MW:29124] derivation welds

 

Yes, this is the purpose of orifice? but usually Olets do not come with 45 deg N U or S D, but the tapping connections are supposed to be in flange as what i have seen, anyhow in your case this is encroached, usually encroachment takes place in your scenario.

 

Basically for SA projects you have to maintain 20 mm or 3 times of the thickness which ever is greater to waive this scenario or if any of those 3 encroached welds have been PWHTed before performing second then exempted.

 

So whats your owner / cleint spec calls for? 

 


Regards,

MOHAMED MUNEEB MAHABOOB

 

 

Date: 2019-02-18 18:31

Subject: [MW:29120] derivation welds

Dear group,

 

Please if you could analyzed the attached image.

 

It´s pipeline B31.8.

 

Constructor at first time, welded tube-flanged joint. Then realized that its necessary have an instrument as showed.

 

The ask is there´re some restrictions for minimal distance between weld joint and derivation in pipe.

 

Please if you could give some reference in design code.

 

Thanks in advance

 

Miroslav Tadic

Integrity Engineer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...