Skip to main content

[MW:29103] Re: Combined WPS meeting EN & Sec.IX Standards.

You can qualify WPS meeting the requirements of ASME Section IX and EN ISO 15614-1 for example. Although it will be very descriptive. E.g. you have to write material grades, material grouping, filler wire grades etc as per both documents.

To qualify, make sure you meet the minimum specified requirements for both. In general ISO PQR qualification is stringent compare to ASME Section IX but ISO is simple to understand with fewer cross-reference while ASME Section IX is full of cross references and require more practical experience.

Regarding testing, EN code call for RT which is not mandatory as per Section IX. EN call for hardness and also specify the limit where section IX doesn't and list is continues. I advise you to go through the EN 15614-1 first and list out the minimum requirements to meet your qualification need and I am sure it will cover most of your ASME Section IX essential variables.

for document writing, make separate WPS for EN & ASME to have a simple and clear WPS.

Thanks & regards
Sandeep Kumar

On Wednesday, February 6, 2019 at 4:03:54 PM UTC+3, john wrote:
Dear Sirs,

Can you please throw some light on WPS meeting both EN Standard & ASME Sec.IX.

Is there any additional test done on test coupon or coupon material needed i.e, impact testing. 

Or WPS is made meeting project requirements only.

Kindly advise.

Best Regards,
John,
08806621979.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...