Skip to main content

Re: [MW:27053] Required electrode for A335 P11 # S316 material

Is it advisable to weld Austenetic SS filler over Nickel base weldments?

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Fri, Nov 24, 2017 at 12:18 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
It is better to use ER NiCr3 instead of Inconel 625 due to its 2nd hardening effect  at High Temperature

Virus-free. www.avast.com

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Fri, Nov 24, 2017 at 11:37 AM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
I suppose it is a Butt Joint. Hence PWHT is required for thickness greater than 13mm for P11 material. Butter the P11 side with ENiCrMo3 with the finished buttered thickness around 5mm, complete the buttering and perform PWHT on the P11 side and weld the remaning joint between buttered bevel & 316 using ENiCrMo3.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Friday, November 24, 2017, 8:08:30 AM GMT+4, Chandra Bhanu Mohapatra <bapunchandra@gmail.com> wrote:


its design temperature is 500 degree centigrade and working pressure is 68 Bar and the joint is pipe to threadolet and pipe thickness is 14 mm..so plz suggest

On Thu, Nov 23, 2017 at 3:23 PM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
It depends on the Design Temperature and any PWHT   if Applicable.

Normally for Design temperatures above 315degC or when PWHT is Applicable

1. Choice one is to use ENiCrMo3(Alloy 625 based) butter the P11 side for around 6-8mm and perform the PWHT and weld the buttered end with the 316 using E309MoL/E309L when design temperature is less than 315degC else weld with ENiCrMo3.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Thursday, November 23, 2017, 1:01:09 PM GMT+4, Chandra Bhanu Mohapatra <bapunchandra@gmail.com> wrote:


Dear Expert 
                       Can somebody help me out to decide the electrode for the pipe welding (Material A335 P11 # S316 ) and Design Code is B31.1

--
tHanks & rEgards
Chandra Bhanu Mohapatra

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.



--
tHanks & rEgards
Chandra Bhanu Mohapatra
8763071417

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...