Skip to main content

Re: [MW:14918] EN 10204 - 3.2 Certificate for Assembled product

Yes Mr.meisam shokri arfaei ,
 
Part 4.2 of EN10204:2004 says:
It shall be permissible for the manufacturer to transfer on to the inspection certificate 3.2 relevant test results obtained by specific inspection on primary or incoming products he uses, provided that the manufacturer operates traceability producers and can provide the corresponding ispection documents required.
 
This sentance is bit confusing..........also the below clause of  specific inspection is also a bit confusing...
 

2.2 - specific inspection:

inspection carried out, before delivery, according to the product specification, on the products to be supplied or on test units of which the products supplied are part, in order to verify that these products are in compliance with the requirements of the order.

it may be applicable to for example a forged product is being made by using a round bar, in that case it may be permissible for manufacturer to transfer the chemical test results of that round bar to final forged rpoduct.
 
But, if you take an example of Valve,
 
See that the casting parts may be made by valve manufacture according to 3.2 certificate, it is ok so far.
 
But, the other parts of a valve like, nut bolts or gasket or non metalic sealings etc. are being procured from the different manufacturers according to 3.1 certificate, How this product can be certify as a whole 3.2 certificate for a complete valve ?
 
If you see the scope of both the EN 10204 & EN 10168, it is limited to raw materials only, at the end of all I think any standard one may follow, but finally the defined scope sumarrise the applicability.
 
 
 


 
On Sat, Jul 21, 2012 at 10:51 AM, meisam shokri arfaei <meisamshokri@gmail.com> wrote:
Dear Sevak,
Part 4.2 of EN10204:2004 says:
It shall be permissible for the manufacturer to transfer on to the inspection certificate 3.2 relevant test results obtained by specific inspection on primary or incoming products he uses, provided that the manufacturer operates traceability producers and can provide the corresponding ispection documents required.
 
From the above part and also "incoming products he uses" I think this standard will not be limited to raw materials. In case of raw materials what do you think about "incoming products"?


 
On Fri, Jul 20, 2012 at 1:48 PM, sevak hiren <hirensevak80@gmail.com> wrote:
Many people think that EN 10204 only covers the type of inspection reports.
 
But they overlook that it is only valid for metallic products/materials and the corresponding manufactures of these materials. Please read EN 10204 again and have a look on the definitions of manufacturer and material.
 
EN 10204 is only applicable for metallic products. A metallic product is not a valve / any assembled product, but - as written in EN 10204 - metal sheets, bars, forgings and castings. EN 10204 can also be used for non-metallic products but it is in any case related to raw materials only.
 
 
On Thu, Jul 19, 2012 at 9:21 AM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Gents,
In case of assembled products an MDR from the manufacturer incorporating MTCs for components used can be the acceptable mode of certification.
Best regards,
Shashank Vagal

--- On Wed, 18/7/12, meisam shokri arfaei <meisamshokri@gmail.com> wrote:

From: meisam shokri arfaei <meisamshokri@gmail.com>
Subject: Re: [MW:14890] EN 10204 - 3.2 Certificate for Assembled product
To: materials-welding@googlegroups.com
Date: Wednesday, 18 July, 2012, 5:30 PM


Dear Sevak
I don't know why you think so, but basically certificate type 3.2 can be use for both row materials and assembled products. Please have a look on part 4.2 of the EN 10204-2004. There mentioned that manufacturer can uses the test results in the 3.2 certificate of his row material directly (without any new test) in the 3.2 certificate of his product.
 
Regards

On Wed, Jul 18, 2012 at 9:05 AM, sevak hiren <hirensevak80@gmail.com> wrote:
Dear Experts,
 
EN 10204 Type 3.2 Certificate is applicable to non-metalic & metalic products like plates, sheets, bars, forgings, castings etc. (Applicable to raw material products only)
 
So, this type of certificate can not be issued for complete assembled products like Valve, Pump, any machine etc.
 
Please let me know your views.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66282127
Fax: +98-21-66282779
 
Please don't print this e-mail unless you really need to. BeGreen!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66282127
Fax: +98-21-66282779
 
Please don't print this e-mail unless you really need to. BeGreen!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...