[MW:14987] RE: 14980] Crosscountry Pipeline construction welding position of Pipe on hill

Dear All,

 

This position is 100%- 6G only no need to doubt in this matter – (for clarification may refer to Sec IX)

 

And 5G will come for the pipe on the ground position – not involved any angular position.

 

Thanks and Regards................?

 

Lakshman Kumar.B|Manager |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BHARAT GOLE
Sent: Monday, July 30, 2012 10:06 AM
To: Material Welding
Subject: [MW:14980] Crosscountry Pipeline construction welding position of Pipe on hill

 

In Crosscountry Pipeline construction what is welding position of Pipe on hill with respect to Welding Procedure as well as Welder qualification. Slope  of hill is around 30 °.

I had always  doubt whether it is  5G or 6G ? In fact I heard always debate on this issue.

Appreciate your expert comments soon.

Regards

Bharat B. Gole

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .