RE: [MW:13978] Heat input value in WPS

Hi Nilesh,

 

Being impact as a requirement, you will have to limit the maximum Heat Input value in WPS as qualified in the PQR. You will have to indicate the values on WPS with upper limit restricted to that in PQR.

 

Thanking you,

Rgds,

 

Prashant

 

 

 

 

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of waman nilesh
Sent: Friday, March 23, 2012 11:07 AM
To: materials-welding@googlegroups.com; materials-welding@goolegroups.com
Cc: wamannp@yahoo.com
Subject: [MW:13977] Heat input value in WPS

 

Dear Experts,

I have question we are doing WPS, PQR & WPQ ( Material- IS 2062 GR B & thickness- 20 mm ) as per EN 15614 standard in which impact is essential.

So which value of heat input is to be mention on  WPS.

 

With Regards,

Nilesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Any views or opinions expressed in this email and its attachments are those of the individual sender except where the sender specifically states them to be that of Lamprell.

This E-mail and any attachments are confidential and may also be legally privileged. If you have received this email and any attachments in error, you are on notice of its status. Please (a) notify the sender immediately by reply email; (b) destroy this email and any attachment, and (c) do not use, copy, store and/or disclose to any person this email and any attachments: to do so could be a breach of confidence. Thank you for your co operation. Please contact the Lamprell IT Helpdesk on ithelpdesk@lamprell.com if you need any assistance.

Holding company: Lamprell plc, incorporated in the Isle of Man, registration number 117101C, registered office at Fort Anne, Douglas, Isle of Man IM1 5PD

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .