Re: [MW:14022] RE: 14017] Renewal &Continunity of welder qualification

Thanks John,
 
I do know about the 6 months renewal of qualification if the welder did not weld.But specificaly I am asking about the welder who is continuing production weld for the last 6 months since his qualification date.
 
My doubts are:
1.I was working with my former employer where we used to get monthly welder performance recod + when a welder complets 6 months from his qualification date ,the contractor QC used to bring a record of his accepted weld joints within the last 3 months so we as a client QC RENEW the welder card by means of  giving company's stamp & signeture so he becoms renewed to carry on welding for the next 6 months.over more, If we find a welder in the field doing welding without Welder ID we suspend him from welding unless his card with him.Even though we know his performance is satisfactory .
2. I am now with new employer where I noticed the welders cards without renewual date .Since then I started to assume that they must be renewed as what I used to do with the former employer.
3.I fully understand that when a welder is welding for the last 6 months doesn't need requalification nor test if his performance is good.the only thing is what I requir is to be provided with Continuty of welder qualification record by means of doing the same as per point No 1 above.
4- I know it would be confusing or not required to do so as long Sec IX dosn't mention such a thing in regard to contractor providin Contiuty of welder qualification to the client in case of welders used to weld for the last 6 month.But Sec IX mentioned in QW.300.3 that welders continuty record to be provided.
5. It would be my own interpretation for the code or my former employer practic in this regard.
 
lastly,
Currently, We have more than one contractor where all are providing us with welder Continuty of qualification record to be signed each 6 month for the welder who are producing weld for the last 6 months.
 
 
Regards,
 
Yahya

2012/3/29 John Henning <jhenning@deltak.com>
If you are going by ASME Boiler and Pressure Vessel Code, there are no
requirements (Interpretation IX-95-38) provided by ScIX on how or when
continuity is to be recorded.  ScIX only states that the weldor is
qualified for 6 months from the last time he used the PROCESS
(Interpretation IX-10-17).

Below is the HSB(r) information on IX-95-38:

ASME Code Interpretations

Status:  Currently Valid
Status Description:


Interpretation: IX-95-38
Subject: Section IX, QW-322, Expiration and Renewal of Qualification
Date Issued: January 6, 1997
File Number: BC96-132
Related Documents:

Question: Is it a requirement of QW-322 for a manufacturer to maintain
records to demonstrate a welder's or welding operator's continuing
qualification for a process from the date of the original qualification
test?

Reply: Section IX does not address how conformance to QW-322 is
demonstrated. Other book sections may address the maintenance of
records.

The above interpretation was transcribed by HSB Code Services from the
official publications [ASME published volumes, National Board,
Eurodyne]. Although every effort was made to accurately reproduce this
interpretation, use of this information should be for research only. It
is strongly recommended that the official published document be used for
Code business.


What I do is scan the weldors records each month and record in a
database the last use of the process for each month.  I include the
drawing number for the work he was involved in.  From this data I can
pull any QA records for the weld if necessary to satisfy a customer or
their inspector.

EN specs are more prescriptive then ASME and require the continuity weld
to be of the same type as the qualifying weld, to be volumetrically
examined, etc.

John A. Henning
Welding & Materials

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of yahya albalushi
Sent: Thursday, March 29, 2012 6:01 AM
To: Materials & Welding
Subject: [MW:14017] Renewal &Continunity of welder qualification

Gents,

For the welder who has been doing production weld for the last 6 months
since his qualification test,Where his company keeping his performance
record.what are the required continuation documents to be provided to
the client in each 6 months? overmore, does his WQT record needs to be
renewed by means of getting stamp of clients QC to validate his
qualification?

Regards,

Yahya
QC(PIPING)
Oman

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...