Hi Dear,
 
           Painting and Coating could be done after hydro testing or pneumatic Testing of the Spools(Welded joints Should be exposed to Atm).

On Sun, Mar 18, 2012 at 6:42 AM, madhan chozhan <madhanchozhan@gmail.com> wrote:
Gents,

Good day.

I need to know whether leak test (hydro or pneumatic) can be done on piping after painting is done on the welds of pipe line?

ASME B 31.3 says "345.3 Preparation for Leak Test
345.3.1 Joints Exposed. All joints, welds (including
structural attachmentwelds to pressure-containing components),
and bonds shall be left uninsulated and
exposed for examination during leak testing, except that
joints previously tested in accordance with this Code
may be insulated or covered. All joints may be primed
and painted prior to leak testing unless a sensitive leak
test (para. 345.8) is required."

"345.8 Sensitive Leak Test
The test shall be in accordance with the Gas and Bubble
Test method specified in the BPV Code, Section V,
Article 10, or by another method demonstrated to have
equal sensitivity. Sensitivity of the test shall be not less
than 10−3 atm·ml/sec under test conditions.
(a) The test pressure shall be at least the lesser of
105 kPa (15 psi) gage or 25% of the design pressure.
(b) The pressure shall be gradually increased until a
gage pressure the lesser of one-half the test pressure or
170 kPa (25 psi) is attained, at which time a preliminary
check shall be made. Then the pressure shall be gradually
increased in steps until the test pressure is reached,
the pressure being held long enough at each step to
equalize piping strains"

here text in green says it shall be left uncovered expect that joints previously tested in accordance with this code(which test to be done for exception and where it is mentioned on code?) but the text in red says it may be primed and painted which looks controversial, kindly advice me what to follow.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,
Padmanabha raju K
0097433459508                                  
Please consider the environment before printing this email

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...