Hi,
1G-CRO qualifies as below for pipe.(As per QW461.9)
 
F - Pipe OD 610mm (24") OD and over
F,H - Pipe OD 73mm 2-7/8") to 610mm(24") OD
 
 please find below the extraction of QW380 for your reference
 

QW-380 SPECIAL PROCESSES

QW-381 Corrosion-Resistant Weld Metal Overlay

QW-381.1 Qualification Test

(a) The size of test coupons, limits of base metal thickness

qualification, required examinations and tests, and test

specimens shall be as specified in table QW-453.

(b) Welders or welding operators who pass the tests for

corrosion-resistant weld metal overlay cladding shall only

be qualified to apply corrosion-resistant weld metal overlay

portion of a groove weld joining composite clad or lined

materials.

(c) The essential variables of QW-350 and QW-360

shall apply for welders and welding operators, respectively,

except there is no limit on the maximum thickness of

corrosion-resistant overlay that may be applied in production.

When specified as essential variables, the limitations

of position and diameter qualified for groove welds shall

apply to overlay welds, except the limitations on diameter

qualified shall apply only to welds deposited in the circumferential

direction.

 



 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 11/19/10, Shadab Alam Ansari <ansari@ghi.com.sa> wrote:

From: Shadab Alam Ansari <ansari@ghi.com.sa>
Subject: [MW:8324] Welder Qualification Range of CRO
To: materials-welding@googlegroups.com
Date: Friday, November 19, 2010, 5:14 PM

If we are making Welder qualification in 1G on CS plate for CRO, What will be the qualification range of pipe dia?

 

Thanking you,

Best regards,

 

Shadab Alam Ansari

Welding Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...