Re: [MW:8321] welder qualification for ASME U stamp vessel

Hi,
As per Sec.IX,Welder Qualification is the manufacturer's responsibility.AI shall review only.AI shall witness only by the the customer's requirement.Please find below the extraction of Sec.IX.

QW-300.2

(a) The basic premises of responsibility in regard to

welding are contained within QW-103 and QW-301.2.

These paragraphs require that each manufacturer or contractor

(an assembler or an installer is to be included within

this premise) shall be responsible for conducting tests to

qualify the performance of welders and welding operators

in accordance with qualified Welding Procedure Specifications,

which his organization employs in the construction

of weldments built in accordance with the Code. The purpose

of this requirement is to ensure that the manufacturer

or contractor has determined that his welders and welding

operators using his procedures are capable of developing

the minimum requirements specified for an acceptable

weldment. This responsibility cannot be delegated to

another organization.

 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 11/19/10, Arnab Bakshi <abaxi1@gmail.com> wrote:

From: Arnab Bakshi <abaxi1@gmail.com>
Subject: Re: [MW:8320] welder qualification for ASME U stamp vessel
To: materials-welding@googlegroups.com
Date: Friday, November 19, 2010, 4:36 PM

As per my understanding, if its a Code Stamp Job, then qualification of welder must be witnessed by AI. Please feel free to correct me if I am wrong.

On Fri, Nov 19, 2010 at 12:43 PM, Priya Deshmukh <piyuwillseeu@gmail.com> wrote:
Dear Santosh,
 
Welder qualification as mentioned below is the responsibility of manufacturer. There is no need to call a Third party to witness the test. The test shall be witnessed by the manufacturer's representative. The procedure for the witness shall be as per your Quality Control manual.
 
Regards,
 
Priyanka Deshmukh.

On Wed, Nov 17, 2010 at 6:07 PM, Santosh Gaikwad <santoshcwi@gmail.com> wrote:
Dear all,
could you please give information regarding welder qualification,i am trying to qualify some new welder for ASME U stamp vessel ,do i need to call third party inspection agency for witness or just i go ahead & run the welder qualification test & get welder certificate endorsed  from AI.

kind regards

Santosh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Priyanka Deshmukh,
Quality Control Engineer,
Transparent Energy Systems Pvt. Ltd.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arnab Bakshi
Welding Engineer,
APIL Durgapur

(Alumnus)Dept. of Metallurgical and Materials Engg
NIT Durgapur
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...