Skip to main content

RE: [MW:8439] HOT PASS

In Duplex stainless steel cold pass technique is required.

Regards

Bharat B. Gole

 






Date: Tue, 30 Nov 2010 00:11:33 -0800
From: rameshnbarot@yahoo.com
Subject: Fw: [MW:8436] HOT PASS
To: materials-welding@googlegroups.com

Dear All,
 
Pl.tell me each and every Process like SMAW, GTAW in SS,CS and LAS required hotpass?
 
In less thickness also?
 
What max.time we can allow for Hot Pass?
 
Waiting for reply...
 
Thanks,
With Best Regards,
Ramesh Barot


----- Forwarded Message ----
From: Shashank Vagal <nach_sam@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Tue, November 30, 2010 11:46:07 AM
Subject: Re: [MW:8430] HOT PASS

Hi Vasu,
The main function of a hot pass is to provide feed to the shrinking root pass weld metal lest it shrink-cracks. The root pass has to penetrate and fill the root gap and initiate the joint. Once it gets a proper metal feed by way of a hot pass, it will do its job well. That is why HP is conducted immediately after the root cleaning operation is over and the root pass is still hot, hence maintaining the same welding set up as used for root pass (and welders) is highly recommended.
It can be seen then why: The hot pass generally uses a higher than normal amperage setting (approx. 10% higher than root amps setting)  and a fast travel speed. The latter to reach all shrinking areas in time. No welding will stop before RP+HP are complete as a minimum.
Shashank Vagal

--- On Sun, 28/11/10, M.Shankar <mails_shankar@yahoo.co.in> wrote:

From: M.Shankar <mails_shankar@yahoo.co.in>
Subject: Re: [MW:8419] HOT PASS
To: materials-welding@googlegroups.com
Date: Sunday, 28 November, 2010, 6:19 PM

Hi Mr. Rao


About & Purpose "HOT PASS"

The surface of a root pass may be irregular, have undercut, overlap, slag incl., or other defects, depending upon the type of weld and the condition of the root pass. The surface of a root can be cleaned by grinding or hot pass.


A hot pass can be used to correct some of the problems caused by a poor root pass. The hot pass may be a hotter than normal filler pass or it may be made without adding extra filler.


A hot pass can be used to correct incomplete root fusion or excessive concavity of the root surface, and improper penetration also.

Eg.1: Improper fusion generally is caused by insufficient heat and temperature for the joint. To correct this condition, a hot pass is used without adding more filler metal.

Eg.2: Concave root surface are generally caused by insufficient filler metal for the joint. To correct this condition, a " hot filler pass" is used to add both the needed metal and heat.


The hot pass should be conducted the same as the first welding process, but depends on your situation. 

Eg. In piping if you use GTAW for root pass, then hot pass should be GTAW-it is preferable. If the welder grind the root to remove defects as stated above, he may remove root completely at any point (accidently), so in this case same welding process is preferred to cover root & your WPS.


The hot pass generally uses a higher than normal amperage setting (approx. 10% higher than root amps setting)  and a fast travel speed.

 

 
Rgds/shankar



From: srinivas rao <ksrvasu@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, 25 November, 2010 12:46:43 AM
Subject: [MW:8366] HOT PASS

Hi Gents,

I have  doubt reg HOT PASS.

1. what is the purpose of doing HOT PASS with more speed and high current?

2. Should the Welding Process used for Root be the same for HOT PASS? If not necessarily then how should we decide?

Thank you All

Regards,

Vasu



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...