Wednesday, April 14, 2010

Re: [MW:4819] Impact requirement for non pressure parts.

Dear Rao,
 
Kindly refer UG-20(f) of ASME section VIII Div-1 (Page 15) .This clears all your doubts
 
 
Regards,
 
V.Ravishanker,

 


From: PAMULA <vasantharao2009@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, 13 April, 2010 2:33:02 PM
Subject: [MW:4809] Impact requirement for non pressure parts.


Dear all,

Is it required to use Impact tested Welding procedure WPS
( supported by Impact tested PQR) to weld vessel internal Parts?

I.e parts that are directly welded on shell/head(non pressure joints).

Vessel is ASME code stamped, Shell & heads base meterials require impact testing as per code.

can any body give code referances (ASME Sec.VIII Div.1/Div.II.

regards
P.Rao

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...