Hi,
Normally, all BFW lines are constructed to the requirements of ASME B 31.1 - Power Piping (clause 136.4.6), which cross refers to the calibration block indicated in ASME Section V.
Regards
Deepak
On 8 April 2010 14:14, Kale, Bhaskar M <bmkale@gmail.com> wrote:
Greeting,
What is the code of constriction, see the inspection and testing clause it may be give details or refer to another standard. Pleas provide the complete information.
Regards,Bhaskar Kale
On Thu, Apr 8, 2010 at 4:00 PM, sreenivas thota <sreeniap2@gmail.com> wrote:
thanks a lot Mr Bhaskar!we r doing HP Piping of thickness of 86mm & 118 mm, dia 600 / 700 mm of Gr A 106C [boiler feed water line]. so for this line we are planning to do UT instead of RT. please advise.On Thu, Apr 8, 2010 at 9:47 AM, Kale, Bhaskar M <bmkale@gmail.com> wrote:
Greeting All,
UT reference calibration block is exclusively depending on the code of constriction.
Generally all ASME code follows the ASME Sec V.
API and AWS D1.1 have their own reference block design and parameters.
If you want ;I can help you on that .please provide your job thickness rage ,material ,product form and code of constriction etc.
Regards, Bhaskar kale
On Thu, Apr 8, 2010 at 11:44 AM, sreenivas thota <sreeniap2@gmail.com> wrote:--dear allhow to make UT reference block? what is the standard as per regulations?
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment