I have one job for marine classification. Material is AISI 4140 and dia id 355.  Our Surveyor is insisting for Longitudinal Tensile Test  and  it cause huge material wastage. Is it approved to go with Transverse direction Test piece for Tensile Test and if so what is the acceptance critiria?
 
Please Clarify!
 
A.Rathinavel
[ QA/QC MANAGER / CSWIP 3.1 ]

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...