Thursday, July 31, 2008

[MW:987] RE: 985] Re: HAZ

Dear Bose,

The difference what you have mentioned that I am also well aware of, but I require some other major difference.

Regards,

Snehkumar L. Mahuri
Lead - Welding / NDE
EPCC 2A, PANIPAT
9215989508

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Rituraj Bose
Sent: Thursday, July 31, 2008 3:32 PM
To: Materials & Welding
Subject: [MW:985] Re: HAZ


Dear Mahuri,

Actually length of HAZ cannot be specified so easily. In any case you
can follow the link to have just an idea for it.

http://www.esabna.com/us/en/education/knowledge/qa/How-does-welding-affect-the-HAZ-of-the-weld.cfm

Regarding your 2nd question I can tell that the Code name itself
identifiy the difference.
API 650 is for the "Welded Steel Tanks for Oil Storage" and API 620 is
for the "Design and Construction of Large, Welded, Low-Pressure
Storage Tanks".

Regards,

R. Bose

On Jul 29, 7:11 am, "Mahuri Snehkumar \(TIPO - QA/QC\)"
<S.Mah...@panipat.ticb.com> wrote:
> Dear friends,
>
> Can someone tell me the exact length of HAZ area after the weld.
>
> Also what is the main difference between API 650 and API 620 codes.
>
> Regards,
>
> Snehkumar L. Mahuri
>
> Lead - Welding / NDE
>
> EPCC 2A, PANIPAT
>
> 9215989508
>
>  image001.gif
> 92KViewDownload

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...