Skip to main content

Re: [MW:31318] Unlisted material is not allowed

Based on the Latest version of ASME Sec.IX (2019) 355NH is listed as P1 Gr.2 as per below snap shot and you can accordingly revise your PQR.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Monday, 17 August, 2020, 02:49:32 pm GMT+7, ViNo Varughese <vinopvarghese@gmail.com> wrote:


Dear KK,

What is the Construction Code? 
Thanks and Regards

VV, Qatar

On Mon, Aug 17, 2020, 10:37 K K <karan.hbl@gmail.com> wrote:
Dear All,

I have received comments from my client as the above subject.
I have submitted my WPS and PQR for approval, please refer below for details.
PQR is qualified with Unlisted material and qualified with according to ASME Sec.IX.
PQR Material - SA 516 Gr.70 to P 355NH.
Please explain to me according to code ASME Sec.IX.
Shall I not qualify WPS unlisted materials according to ASME Sec.IX ?
or Unlisted material is not allowed according to ASME Sec.IX.
The propose of qualification is for stack supporting structure, seal welding of convection to the radiant section.
Please looking your favorable replay to my query.

Thanks and Regards.
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/047ccc24-c19e-45fd-b511-efa8eaba1b17n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7Ard4LhVjbnzz0Akm6AvfpYBOAd1rJY3bGeWZncoLmcow%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...