Re: [MW:31253] Combination of PQRs

if f no is same u can, but it overmatching if u use incoloy filler. u can use NiCrMo3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sun, Aug 2, 2020 at 9:54 AM Customer Care <bricenori@hotmail.com> wrote:

Dear Prasad,

It seems to me that your proposal is not valid because the INCOLOY  825 alloy belongs to the family of nickel base alloys with filler metal within SFA 5.14. (for example ERNiFeCr-1).

 

904 L is a high alloy austenitic stainless steel and must be welded with filler metal of the same composition within SFA 5.9 (ER385) and also to weld the SS 317 / 904L combination.

 

You should prepare WPS with PQR for this 904L alloy.

 

Regards,

 

Ramon Briceno / Metallurgical Engineer -Oil & Gas

www.linkedin.com/in/ramon-briceño-976265b5

 

Sent from Mail for Windows 10

 

From: prasad loke
Sent: Saturday, August 1, 2020 7:20 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:31251] Combination of PQRs

 

Dear Sir,

 

Greetings !

 

We are in need your expert opinion on following issue,

 

We have WPS/PQR for Incolloy 825-Incolloy 825 ( P number 45)----Filler used for same is from SFA 5.14

Now We have a requirement of SS904L to SS904L welding.( P number 45)---Where recommended filler is ER385 with SFA 5.9

 

If we make WPS with filler from SFA 5.14 for this (SS904L to SS904L) welding as P number is same, can it be supported with existing PQR of Inc-825 to INC-825 ?

 

Thanks in advance.

 

Regards

Prasad Loke

 

On Mon, Jul 27, 2020 at 1:03 PM K K <karan.hbl@gmail.com> wrote:

Hi Experts,

 

"Good Morning"

 

According to my line classes, I required NACE+HIC+PWHT Wet H2 services.

What is the test shall be conducted according to the standard to meet the requirements?

 

I have one PQR with NACE+PWHT+Wet H2S services, but not HIC test.

In addition, I have qualified one HIC tested PQR without PWHT no other lab test certificates, shall I combined this PQR to the above requirements( NACE+HIC+PWHT+wet H2S).

For your information, the HIC test is an additional requirement of our specifications.

Please looking your feedback on my above query.

 

Thanks and Regards

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f1d53635-4e0f-4fe5-a0cf-ec93a8d2d87bo%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAS23S%2BpsvrtaQp%2B12MGvpjTP4jvPe5KrgK4JWyQXMjUabc1Lg%40mail.gmail.com.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL0PR03MB4243DEA528576FEC3B033578AA4F0%40BL0PR03MB4243.namprd03.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOsjZNyttY2TJCeAznuRwCuPta2SEWfPcK8BOtRwTECMA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...