Skip to main content

Re: [MW:31341] Re: Impact test requirements for LAS

agreed, but need to consider startup/shutdown (or streams where continuous flow is not present) conditions also during design

On Thu, 20 Aug 2020 at 09:19, Customer Care <bricenori@hotmail.com> wrote:

Yes, it is understood, in an arctic environment like Russia, for example, the low temperature excursion is present in the services. But, if the process where the SA-335 P9 pipe is installed serves a furnace, boiler, reactor or incinerator operating in the creep and oxidation range; typically, the engineering specification indicates pipeline protection with traces of heating and thermal insulation that suppresses freezing.

 

Ramon Briceno/ Corrosion-Materials & Welding Engineer

 

Sent from Mail for Windows 10

 

From: Raghuram Bathula
Sent: Wednesday, August 19, 2020 1:16 AM
To: Materials-Welding
Subject: Re: [MW:31338] Re: Impact test requirements for LAS

 

Please go thro the previous discussions on the subject

These conditions are applied in particular where ambient temp is very cold, for e.g Russian region MDMT can go upto -50 deg c.

 

 

On Wed, 19 Aug 2020 at 09:58, Paidi <bobsuresh24@gmail.com> wrote:

Well said... Exactly.. Coarse grained steel does not required Imoact test requirements unless until service is different than normal... Cryogenic and all 

 

On Wed, 19 Aug 2020, 09:39 Customer Care, <bricenori@hotmail.com> wrote:

Dear Kiran,

 

It is rare that a low Cr-Mo alloy steel such as Group P5B is required to have an impact test at -29 C in its weld.

These steels are resistant to high temperatures of approximately 470 C to 650 C. So for what impact test? Structurally, for high temperature service a steel with a coarse grain size ASTM 4-5 (creep and oxidation resistant) is needed; and for low temperatures, tough steels with fine grain structure ASTM 8-9 are needed, which are suitable for cold service> -29 C to -45C.

 

The steels grouped in P5B are coarse-grained.

 

ASME B31.3 does not call for impact test at this temperature -29C. First of all, Kiran you must check the service temperature range of this pipe and its welding. What is approved in the Customer's specifications? I think your Customer  is wrong. Talk to him.

 

Regards,

 

Ramon Briceno/ Corrosion-Materials & Welding Engineer

 

Sent from Mail for Windows 10

 

From:
Sent: Tuesday, August 18, 2020 3:36 AM
To: Materials & Welding
Subject: [MW:31328] Re: Impact test requirements for LAS

 

Dear Experts,

 

Please I need your answer to my above query. 

 

My client has mentioned the above 25 mm Impact test would be required, in accordance with B31.3.

 

Question: Are materials, for which a temperature of −20°F (−29°C) is listed in the Minimum Temperature column of

Table A-1, exempt from impact testing for any combination of thickness and temperature above −20°F (−29°C)? Reply: Yes.

The minimum temperature in our scope is not below minus 29°C. If B31.3 calls for impact test within this temperature.

 

Your feedback is very important to me.

 

 

On Tuesday, July 28, 2020 at 10:12:01 AM UTC+5:30 K K wrote:

Dear Experts,

 

Please look into my query, please give me your response on my doubt.

 

Thanks

 Kiran 



On Monday, July 27, 2020 at 11:29:05 AM UTC+5:30, K K wrote:

Hi Experts,

 

"Good Morning"

 

My query has below.

 

Help me to prepare pWPS.

Process : GTAW +SMAW

Material : P.No - 5B   

ASTM A335 Grade P9.
Pipe Size - 16" Sch-60.
Thickness: 16.66 mm
Thickness range: 5mm to 33.32 mm
According to ASME B31.3 Table 323.3.1 shall I required an Impact for the above-mentioned thickness and material.
As per my knowledge, the above 25 mm impact test would be required. 
How I can find according to line class where impact test required or not.
If a minus 29° C impact test not required for LAS. 

When we shall consider the impact test exemption. 

 

And regarding consumable for P No- 5A 

ASTM A335 Grade P22

 

if I use ER90S-B3 ok or shall I use ER80S-B3 because my client suggest me to use ER80S-B3 please clarify way?

 

Thanks in advance 

 

Regards

Kiran

 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e850f3f0-ffab-4097-b05e-5e8063cc163fn%40googlegroups.com.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL0PR03MB4243D86E83ED1D6C00059921AA5C0%40BL0PR03MB4243.namprd03.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA%3D1_-xrRM5VdAO1EZe4LPiXQENTG0i0qv3d_ooFsqbGVW%3DM%2BA%40mail.gmail.com.


 

--

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DvFmxayOeaVTRaR8PwmDgg9u6KDc38M%3DeROX1SHmqoWw%40mail.gmail.com.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/SN6PR03MB42542AE5F2745253494F30F1AA5D0%40SN6PR03MB4254.namprd03.prod.outlook.com.


--

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnMKQhbwQcaNGVBf_PPXx813Ygz89XPBd5mxtrS4v5s1A%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...