Skip to main content

Re: [MW:31349] How to check Argon Gas Purity?

Dear All

Checking Impurities in Argon gas cylinder is still a secret with the Gas manufacturers.

We need to check following impurities in Ultra high pure Argon gas # CO2, CO, oxide of nitrogen, hydrogen, nitrogen, hydrocarbons, sulphur compounds, mercury, chlorine.

But all Argon gas manufacturers in India are able to check only dew point, moisture and oxygen .

Can anyone help please ..

Regards

Prem Nautiyal
Cell 9769316004

PREM S NAUTIYAL
CELL : 9769316004





From: "PREM SHANKARDUTT NAUTIYAL"<prem_nautiyal@rediffmail.com>
Sent: Sat, 22 Aug 2020 21:14:18 GMT+0530
To: "materials-welding@googlegroups.com"<materials-welding@googlegroups.com>
Subject: Re: [MW:31312] How to check Argon Gas Purity?

Shaw meter will only measure the dew point..

How to measure other impurities like moisture, oxygen, hydrogen, oxides of nitrogen, chlorine, sulphur, etc ?

Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9769316004





From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Mon, 17 Aug 2020 11:33:00 GMT+0530
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:31312] How to check Argon Gas Purity?

Shaw meter available.
But always better weld in a piece and then proceed to job. Due to improper cleaning base metal also will result this black mark

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Aug 17, 2020 at 10:48 AM TRIVIKRAM <trivikram977@gmail.com> wrote:
Dear All,

we are doing Aluminium alloy welding by (TIG) process, during welding we observed black mark around the welding for some argon gas cylinders.

Please suggest how to check the gas purity level and any instruments / gauge are available.

Thanks & Regards,

Trivikram

On Friday, April 4, 2014 at 9:23:35 AM UTC+5:30, prabhu wrote:
Dear All,
 
I my doing work on SS material 316L , ensurinig clean and dust free area and surface but enable to rnsure the Argon gas purity.
please guid me how to ensure the gas .
Or is there any divice to check the Argon gas impurities.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/5106e351-0d94-4a13-bcc3-16091e6f8d83o@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/CAJzm4ePwCLxPry9MUoHJ_8zRcwPMAP==BHaRVSh-HX75m 346A@mail.gmail.com.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1598245139.S.93642.autosave.drafts.1598245605.19225%40webmail.rediffmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...