Re: [MW:31369] Supplementary Essential Variables

This clause is applicable when Notch toughness tesing is specified.

Please Refer  ASME Sec IX clause No. 251.2- Essential variables are those in which a change, as described in the specific
variables, is considered to affect the mechanical proper�ties of the weldment, and shall require requalification of the WPS.
Supplementary essential variables are required for me�tals for which other Sections specify toughness tests and are in addition to the essential variables for each welding
process.


On Sun, 30 Aug 2020 at 5:43 PM, udaya bhaskar <dusroni@gmail.com> wrote:
Dear Experts,


Please Can you clarify to me the above highlighted point "T limits toughness". 
This point Where is and when is applicable these Supplementary Essential Variables in WPS.
Will This Clause be applicable in water station piping WPS at Gulf countries?
Material : API5L-PSL2





--
With Regards

Udaya bahaskar.D

+919676270121








--


https://materials-welding.blogspot.com/


https://www.linkedin.com/groups/122787


---


You received this message because you are subscribed to the Google Groups "Materials & Welding" group.


To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.


To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3ROgt2d1_hs8pgoZqKd5EUjgd7quAqH8h-8z%2BnBfr2%3Dd0A%40mail.gmail.com.


--
Regards,
Kundan Ahirao

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALY5PPju4AhLuvZ4R8XakHb8_uPrWwd_xhL3ppukj826BuzK%3DQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...