Skip to main content

[MW:31361] RE: 31360] Re: As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1 and API RP 582

Hi KK,

 

What's the design  code ? ASME Sec VIII , DIV-1 or ASME B-31.3. Looking at the text below, it sounds  Sec VIII, DIV-1 is the design code.

Look at this curve and the exemption clauses for more clarifications. If this curve exempts BM/thickness from impact test , then weld/HAZ should be exempted from impact also.

 

Thanks.

 

 

Pradip Goswami, P.Eng, IWE

Consultant-Welding-Metallurgical Engineering

 

Cell & Whatsapp-905-9793232.

Personal:pgoswami@rogers.com

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of K K
Sent: August 28, 2020 6:45 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:31360] Re: As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1 and API RP 582

 

 Dear Experts,  

  
Can I get a response from you?

 

According to  ASME Sec.8, and MDMT is 5°C.

 

Please send me your valuable reply to my doubts.

 

Thanks and Regards

KK

 

 

On Wednesday, August 26, 2020 at 9:47:06 AM UTC+5:30 K K wrote:

Dear Experts,  

 

Impact testing requirements for  Equipment Anchor Chair to top plate/wash welding, base plate, and plug welding.

According to ASME B31.3  above 25mm impact test required.

So for that,  I have restricted to my thickness range 5.00mm to 25.4 mm in WPS.

But Now my requirements for welding Equipment Anchor Chair to top plate/wash welding, base plate, and plug welding.  up to  32.88 mm,

For the 32.88 mm thickness, I have to conduct an impact test or not required impact test 

Process - SMAW.

P No - P1.Gr.No- 1 to P1 Gr,1/2

Thickness range - 5.00 mm to 32.88 mm.

Material - ASTM 516 Gr.60 to ASTM Gr.70

 

As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1, and API RP 582according to mentioned code required Impact test or not?

 

Thanks in advance  

 

Regards

KK

 

 

 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/49f11814-bb8f-434c-8da9-9551a4ad71a9n%40googlegroups.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...