Skip to main content

Re: [MW:30558] Re: PQR mentioning position 3G and our WPS stated 1G

WPS is basically a Base line document used by the Welder and Welding Supervisor which need to be Approved by the Client.

Client will check with the PQR (submitted by you to client) and verify the Applicable code to approve the WPS which will be used by the welder cross-checked by Welding Inspector.

Hence revisions to be made in the WPS according to your shop floor requirement.

Thanks & Regards

J.Gerald Jayakumar




On Friday, February 28, 2020, 01:15:16 PM GMT+7, Rash <tiamlord@gmail.com> wrote:


IF position not an essential variables, why need to change WPS  1G and add 6G position?




понедельник, 20 октября 2014 г., 16:29:28 UTC+5 пользователь dili...@gmail.com написал:

If your Code is ASME and if your project specifications do not include any additional requirements, then you may proceed as follows:
Position is not an essential variable for WPS qualification, so you do not need a new PQR.
You draft a new WPS based on the essential variables of the existing PQR and you include also the position 6G.
Then you can qualify the welder

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

Inactive hide details for Mohammed Zakeruddin ---20/10/2014 08:40:47---Dear All, Kindly advise,Mohammed Zakeruddin ---20/10/2014 08:40:47---Dear All, Kindly advise,

From: Mohammed Zakeruddin <zaker....@gmail.com>
To: material...@ googlegroups.com
Date: 20/10/2014 08:40
Subject: [MW:22147] Re: PQR mentioning position 3G and our WPS stated 1G
Sent by: material...@ googlegroups.com




Dear All,
Kindly advise,

1G Qualificaiton is mentioned on WPS & PQR and if we want to qualify the welder on 6G position, do we need to prepare new WPS and PQR or only PQR and WPS (1G) be the same....

Khan....

On Tuesday, November 16, 2010 11:27:05 AM UTC+4, israr wrote:
    Dear,
    You just delete position 1 g from wps and write All,
    As per ASME Section IX if WPS is qualified in any one position of 1G
    to 6G it is qualify for all the position.
    Then u can attached nos of PQR with dirrent position following the
    same WPS.

    Regards
    Israr Ahmed
    Tata Projects Ltd.India
    +919930308261

    On Nov 11, 2:35 pm, Zulfan <zul...@insing.com> wrote:
    > Dear all,
    >
    > please advice in our PQR mentioning position 3G and our WPS stated 1G
    > is the WPS able to apply or need to run again PQR again?
    > code ASME sec IX
    >
    > Thank
    > zul

--
To post to this group, send email to material...@ googlegroups.com
To unsubscribe from this group, send email to material...@ googlegroups.com
For more options, visit this group's bolg at
http://materials-welding. blogspot.com/
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@ googlegroups.com.
For more options, visit
https://groups.google.com/d/ optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer. bureauveritas.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aeef7d9d-e9b6-40ec-9f0b-d98e790ee499%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...