Re: [MW:30523] Re: Impact Test

70N - Yes, normalized plates,, Just overlooked ! 

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Thu, Feb 20, 2020 at 11:57 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
70N??

On Wed, 19 Feb 2020 5:35 pm Ramesh, <rameshkannandevaraj@gmail.com> wrote:

I presume there is no specific service requirements and plates are normalized

 

As per Figure UCS-66M of Sec 8 Div.1, The plate material 516 fouls under curve D. the impact testing is exempted up to -48°C .

 

Reg welding, The electrode E7018-1 is guaranteed impact values at -45°C. Refer Table 3 of SFA 5.1.

 

But its better to have impact tested PQRs for company future use. 

Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Feb 19, 2020 at 3:39 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AMkqLQr%2BV0KXTtf%3DG%2BX03SpPg8z92ePJqHXO0PJpZctg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcHs5XyOXpGeyN2r%2B%3D2C6Yej%2BWoRt2AucX%2Bjh_6xN4eTew%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOxFw8YR6iF1yOFoBR%2BHiwSdUL39SFU7%2Bo6pm8mt0jqZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcGuQ2tKiYrvbuuQaKd1PP58TaGbXoN6%3DDoowhJg6LHk-g%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...