Skip to main content

Re: [MW:30461] Re: Time between root pass and hot pass

Dear, 

Even if it is mentioned in code, if it is not in WPS or the project specification, then you are not required to do it mandatory. An engineering query can be raised and this can be considered as interruption of welding. In such case, the following methods can be suggested. 
1. Visual examination of root to check out for cracks 
2.DPT to check for fine cracks open to surface. 
3. Radiography to ensure no cracks inside.
Hope this helps.

Regards, 
Charles  Jacob 
Welding Consultant
Magnum Consultancy Services
+91 7034331779  

On Mon, Feb 10, 2020, 12:46 PM <tahirkaimi@gmail.com> wrote:
would you please guide me that can we left the joints after hot pass and complete the joints next day.

On Tuesday, 15 May 2012 18:25:43 UTC+5, jesti fer wrote:
Dear all,
We are doing 20" pipe line project with API 5L Gr.B material as per B31.4, Welding process SMAW (E6010 for root and rest with E 7018, both are up-hill) our welder welded one joint root pass and he kept this joint for long time. But our Qc instructed to cut and re-weld the joint. But the time between root pass and hot pass not mentioned in approved WPS and client specification also.
It necessary to cut and re-weld?
It is mentioned any were in the code (ASME or API)?
 
Please help me,,
  
Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7cecaded-0dcc-453f-acdc-fcf382f26300%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4BOf-ve6bjYbwduS_z%3D43_817sRJ8tQjoyQ1eb5RepRCA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...