[MW:30467] Qualification of Hard-facing overlay welding using Ultimet

Dear Experts,

 

We have a qualified PQR and WPS for Hardfacing overlay welding of Stellite 6 to C276 (UNS N10276; P-no.43 according to ASME IX QW-422)

 

The following applies to stellite:

CLASSIFICATION

AWS A 5.21: ER CoCr-A

EN ISO 14700: RZ Co2

DIN 8555: WSG 20-G0-40-CTZ

 

Used process: GTAW

 

Now the client wants us to do Ultimet hard facing overlay welding on Hastelloy C276.

 

For the Ultimet solid wired we found:

CLASSIFICATION

AWS 5.21: no class

UNS R31233

ASTM: B815

DIN: W.Nr. 2.4681

DIN CoCr26Ni9Mo5W

 

According to ASME IX, QW-432, all A5.21 is F-no.72 Filler wire

 

QUESTION:

Is it allowed to use above mentioned PQR (F-no.72 to P-no.43) to make a WPS for this job, or do we have to qualify a new PQR?

 

Looking forward to your valuable response,

 

Best regards,
Hans Smithuis
Valve Specialist / Welding Coordinator
Red Point Alloys BV     email    hans@redpoint.nl
Radonstraat 2   phone   +31 79 363 2070
2718 TA  Zoetermeer     website
www.redpoint.nl
The Netherlands           


 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...