Skip to main content

Re: [MW:30533] HIC Resistant Material - EIL Specification

Hi,

I am not sure about EIL requirements.

Normally Forgings and Seamless pipes do not require HIC testing requirement as the these production methods eliminate many discontinuities(impurities) which cause HIC.

Only plates are to be tested for HIC testing to Client Specifications or to ISO TM0284. Pipes rolled from plates also require this testing.

Regards,
Albert R


Sent from Yahoo Mail for iPhone

On Friday, February 21, 2020, 2:20 PM, sagar bogwad <sagarbogwad@gmail.com> wrote:

Dear Experts,

Need your expert advise on below :

Background :
Equipment data sheet specifies HIC resistant material to be used.
And applicable EIL specification 6-79-0013 R1 (Material requirements for Carbon steel components used in Sour service for petroleum refinery environment)
I understand these specification calls for HIC testing of Plates & Rolled products(pipes fittings made from plates) only.

Question :
Does EIL Specification 6-79-0013 R1 calls for HIC testing of components other than plates & rolled products such as Forgings, pipes, fittings, fasteners as well?

Kindly confirm with clarifications for better understanding.


Best Regards, 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiDOxk%3DNOyKmTeY%3DdPa1WTvc%2Bw51q0M1AbsANrqFL5fXwzPhg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...