Skip to main content

[MW:30461] Re: API 650 & 653

Thanks Kesava,

Can you please explain me more regarding corrosion or defect, inspection methods and acceptance criteria.

And for your information i don't have experience in API Tanks.

So for please explain me in details. And you have not addressed API 653.

And thanks for your reply.

On Monday, February 10, 2020 at 12:46:30 PM UTC+5:30, k7moorthi wrote:
Hi Kiran,

Refer API-650_2014, 
Section-4 (Clause  4.1.2 , 4.1.3 & 4.1.4) for all materials.
Clause :- 4.2 for Plates material specification requirements.


With Regards,
Kesavamoorthi.R.



On Saturday, 8 February 2020 13:39:40 UTC+3, K K wrote:
Dear All,

I hope I will get good response from Material & Welding experts.

The requirements for base materials in Tanks. 


If base material (plates during receiving inspection) shows some corrosion or defect, which ones would be the recommended inspection 


methods and acceptance criteria.


May be is included in API standard or in ASTM standard for each material. (For example A516 gr.70 or A283 gr.C).


Please which code shall i refer, please give me response in details.


Thanks in advance.


Regards

Kiran 


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c7c2abe-e036-4bda-a114-3275c606d1ea%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...