Skip to main content

Re: [MW:22827] Welder Qualification

The first and main document should be used as a reference is a contract. If it mentioned in the contract documents, there is no problem. You will find the acceptable codes, standards, specs., procedures and any other guideline in those documents.

But generally in case of any conflict, the procedure cancels the spec, and the spec cancels the code or standard. Because the procedures have more details and adaptation compare to specs and specs also have more details and adaptation compare to codes and standards.

Regards

On Mon, Feb 9, 2015 at 10:51 AM, Ludmila MANUEL <ludmila.manuel@total.com> wrote:

Dear experts,

 

Please can you give me your advise

 

Can I accept a job in process (Process piping) ASME B31.3 and spec ask for welder qualification as per ASME IX and the welder is qualified as API 1104 (Pipelines)

 

Is there any restriction?

 

thanks

 

 

Ludmila MANUEL

QC Inspector

TOTAL E&P ANGOLA

DT/EPT/ MHSAQ/QUA
Tel : +244 222 67 3443

Cell:+244 912 641 670
Email:
ludmila.Manuel@total.com

 

Mailing Address:

TOTAL E&P Angola
Rua 6 IL 6 B.I SONILS, Boavista Office B.I 100-01
1
Luanda - Angola

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1B0224B9A78AB34285E27B011195A0469E7D829F26%40AOEPTTA-EG11.main.glb.corp.local.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMts6tFyeBbfW6k2T26783cTAYLbo5w4xg74MNhu-tEjiCA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...