[MW:22871] Acceptance of PMI

PMI results should be considered only for validation and not as acceptance. If any doubt in chemical composition grind off few sample and send it to lab for chemical analysis.

Regards 
Mohan

On Friday, February 13, 2015, Saravanan Sornam <saravanshyla@gmail.com> wrote:
Dear Experts,

based on the below conversation, 

incase a fabricator owns a PMI machine,

what will be the Tolerance for chemical elements ( base metal and Weld metal )  and what is the accuracy level for calibrating the PMI machine.

Regards,
Saravanan

On Fri, Feb 13, 2015 at 12:37 PM, pradip kumar Sil <pradipsil@gmail.com> wrote:
Follow PFS standard, 10% bilateral tolerance on parent material & 12.5 % tolerance  on weld material. 
Chk composition on ASME SEC II

On Fri, Feb 13, 2015 at 5:12 AM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear Experts,

We have done PMION weld joint of INCONEL625 i.e. ENiCrMo-3
Found
Ni -61, Cr-24.6, 25.6, Mo-8.5, Nb -3.37,

Now, As per procedure & code i. e.
Sec II C Cr range is 20-23 given
all other elements are in range.
And PMI analyzer also display Inconel 625.
Please confirm whether it is acceptable or not i.e. chromium %

Best Regards,
Mohit Aggarwal.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPOtBHVu5HvuVxdG24WR3uCSsH5sXQkAGkf7C1eLug-r0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DqR-d5rm49p7kE9vPk6i1Qw9iyzBL%2BPq_ufxjCVTEiTw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJ1XUvsWURcPmPaa7jrijoLD9wm2xZFd3%3DMS4s3u2PW%3DA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
Regards
Mohankumar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEQCnx1wPyuCggqiDU80kGi6z6gB7aJMrfWSwZbh2xOaEFSU1Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...