Re: Fw: [MW:22886] Rechniques for checking internal surface of piping 12" and 16" for natural gas supply

for a continuous pipeline you can use LRUT online and again boroscope offline.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,
 API653, NACE CIP-2, LEEA Registered Engineer.

On Mon, Feb 16, 2015 at 8:50 AM, Mohammed Ghani <ghani386@gmail.com> wrote:
Dear,

its a 40 mtr. continous in service pipe line. i need two options.

1. with out shutdown any chances of internal surface inspection?.
2. with shutdown what are the various types of instruments available for checking internal surface of piping of 40 mtr. length.

Thanks and Regards,
Mohammed Ghani.

On Mon, Feb 16, 2015 at 7:00 AM, 'smkabeer ahamed' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear friend,

snake eye -iii is one type of instrument  used to check internal surface defects,welding defects.vt-level-ii engineers used that instrument.you can approach ndt agency to collect  that instrument and inspect that piping.

Thanks and regards.

S.M.Kabeer ahamed
chief engineer
M/S.QUEST -BANGALURU
INDIA


On Monday, 16 February 2015 8:41 AM, Kunal Patel <kunal.patel13683@gmail.com> wrote:


Dear friend,

For checking internal surface of piping, we can use Borescope or Fiberscope. This is an instrument, which is available in market or vendor places.

Regards,
Kunal Patel
BVIS Ahmedabad.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2a5bc249-f4b9-4c05-9b56-db67ce9d0598%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/101087077.2960395.1424059210045.JavaMail.yahoo%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjNPvBL%2Bi%2BAo1_rQBdrCxfsd0cdVPwu1%2BxO3C5UmeMjmA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKygcK6UwQsfp6uNvZ0q4F%3DzfgROc2_0G5r2OHNx5q3q7pw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...