RE: [MW:19110] Change in Supplementary Essential Need re-qualification?

Yes if THERE IS NO Impact test required.

 

Thanks,

HEMANT SUTHAR

IWT

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: 29 October 2013 14:28
To: materials-welding@googlegroups.com
Subject: Re: [MW:19108] Change in Supplementary Essential Need re-qualification?

 

Yes it does

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector
Prelude FLNG ASME Subject Matter Expert

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS

Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Korea cell phone: +82 10 2777 8922


Ezat Adel ---29/10/2013 10:57:21---Dear Experts, i need your clarify that the changes in material group number with the

From: Ezat Adel <ezatadel2008@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Date: 29/10/2013 10:57
Subject: [MW:19105] Change in Supplementary Essential Need re-qualification?
Sent by: materials-welding@googlegroups.com





Dear Experts,

i need your clarify that the changes in material group number with the
same p number need another welding qualification or not.

my case i have WPS for A312  grade TP 316, P no. 8 , group no. 1 to itself.
it's right to use it to weld  A312  grade TP 310s, P no. 8 , group no.
2 to itself.

Ezzat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Re: [MW:30066] Diameter qualified for set in nozzle

refer IX-80-67 On Mon, 16 Sep 2019 at 12:56, Muhammed Ibrahim PK < ibratech@gmail.com > wrote: Gents,  Is there any interpretation available for set in type nozzle welding diameter not essential variable for welder qualification?. Reg --  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmhNusk1TKk-%3D0t%3Dfcyz0NnpVGvN3Wisj1mL%2B9aoAoRnA%40mail.gmail.com .

Re: [MW:30053] Re: pwps format required

Any body can clarify about  pre heating of ss  pipe joints  in -25°c climet  site work... need pre heating  or no... waiting for your valuable replay On Fri, 13 Sep 2019, 5:39 pm Bien_ND / weldinginspections.net , < bck055@gmail.com > wrote: Hello, get free WPS and PQR format at 1- WPS for SMAW: https://lnkd.in/fevanEM 2- WPS for GTAW: https://lnkd.in/fzYnQKP 3- WPS for GTAW + FCAW: https://lnkd.in/fxMryha 4- WPS for GTAW + SMAW: https://lnkd.in/fQVJFN7 5- WPS for GTAW + SAW: https://lnkd.in/fjW6gvq 6- WPS for GTAW + GMAW: https://lnkd.in/fJ_mzK4 On Wednesday, September 11, 2019 at 3:51:59 PM UTC+7, Dharma dattu wrote: Hello All, we need to establish a wps with SMAW + SAW process, can you share the format. my doubt is will it be called as welder qualification  or (welding operator qualification). Regards, DD -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Go...