Re: [MW:19079] Re: Comparision of UT & RT ( Justifying UT )

Gents,
I would suggest first UT scan for root zone preferably with 70 deg probe of as high frequency as feasible. If any flaws exist in root, unless they are attended to, all further inspection activity is not justified.
 
With Bets Regards,
Shashank C Vagal     



On Friday, 25 October 2013 4:48 PM, Tahir Olmez <tahirolmez@gmail.com> wrote:
RELATIVE ADVANTAGES AND WEAKNESSES OF RADIOGRAPHY VS ULTRASONIC, TWO COMPLEMENTARY TECHNIQUES Ultrasonic and radiographic examination methods are complimentary and are not directly comparable or equivalent. Depending on flaw type (i.e., volumetric or planar) and orientation, ultrasonic examination may be superior to radiography or vice versa. Radiography is most effective in detection of volumetric type flaws (i.e., slag and porosity) and detection of planar type flaws (i.e., lack of fusion and cracks) that are oriented in a plane parallel to the x-ray beam. However, radiography is limited in detection of planar flaws not oriented parallel to the beam. In contrast, ultrasonic examination is very effective in detection of planar type flaws that are not oriented in a plane parallel to the sound beam .... Finally, ultrasonic examination is capable of detecting volumetric type flaws such as slag or porosity but is limited, compared to radiography, in ability to characterize volumetric flaws. The proposed alternative ultrasonic examination requirements and provisions address the known limitations of the ultrasonic method to ensure both planar and volumetric flaws in all orientations are detected and properly evaluated. First, examination using two angle beams (i.e., 45 and 60 degree nominally) or a procedure qualified on 100% of the weld volume in accordance with the performance demonstration methodology of Section XI, Appendix VIII is required. Second, examination scans in two directions perpendicular to the weld axis and two directions parallel to the weld axis or examination scans as qualified on 100% of the weld volume in accordance with the performance demonstration methodology of Section XI, Appendix VIII is required. Third, to ensure laminar type flaws are detected, a supplemental examination using straight beam is also required. Finally, if an indication, such as slag or porosity, is not characterized as volumetric, the indication will be characterized as a planar type flaw and evaluated in accordance with the acceptance criteria of NC-5330. The acceptance criteria of NC-5330 specify acceptable lengths of indications only and do not differentiate between planar and volumetric type flaws. Most importantly, planar type flaws such as cracks, incomplete penetration, and lack of fusion, which are rejectable by NC-5330 for any size, are more readily and properly characterized by ultrasonic examination. In addition to the effectiveness of the proposed alternative, use of ultrasonic examination in lieu of radiography will provide a significant reduction in personnel radiation exposure during refueling outage maintenance work. Also outage duration and costs will be reduced by allowing parallel path work to progress uninterrupted during examination of welds. Finally, the personnel safety risk of inadvertent or accidental exposure and also the normal anticipated exposure associated with transporting, positioning and exposing a source for radiography is eliminated. Source: D. Naujock et al. (NRC Office of Nuclear Reactor Regulation), http://www.nuclear.com/archive/2003/07/13/20030713-002.html Callaway-1 10-yr pipe test ISI - UT approved in lieu of radiography , nuclear.com info nugget 20030713-002, July 1, 2003] Tahir Bilge Ölmez International Welding Engineer

On Friday, July 4, 2008 9:53:26 AM UTC+3, vhr...@gmail.com wrote:
Dear All,
 
We awared Hydro power project. There is specifically requirments of NDT method RT for all weld joint ( i.e for all class of joint ).
 
We never used RT in normal practice for all project. Now for convince to client We required comparision sheet between RT & UT to justifying UT is better than RT.
 
Request to send Comparision of RT & UT. Please send comparision & revert back soon. We have to submitt QAP urgentely.
 
 
Regards,
 
Vikas Rana
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...