RE: [MW:19060] -40F (-40C) impact qualification of 1-1/4Cr 1/2Mo (P4)

Sorry, the material design temperature of the 1-1/4Cr 1/2Mo (P4) limit between -20°F to 1000°F  and not is designed to work to -40 °F. Remember this low alloy steel is selectionated to systems that driver high temperature service because the principal alloying elements are Cr and Mo, so this low alloy steel have resistance to the oxidation and creep. Use it in low temperature like -40°F  not is good idea, it prone to fragil fracture during the impact testing.  

Sincerely,
Ramon Briceno
Metallurgical Engineer.

Date: Wed, 23 Oct 2013 13:57:13 -0700
From: jhenning@deltak.com
To: materials-welding@googlegroups.com
Subject: [MW:19056] -40F (-40C) impact qualification of 1-1/4Cr 1/2Mo (P4)

I have a customer requiring -40F (-40C) impact qualification for 1-1/4Cr 1/2Mo material (ASME Sc IX).  Design and fabrication is required to be in accordance with ASME Sc. VIII, Division 1.  Weld thickness is approximately 1-3/4 in. (45mm).  It is anticipated that only SAW and SMAW will be required.  While I have a number of procedures qualified at -20F (-29C) it would appear that they are approaching the DBTT for the weld metal and HAZ in most instances.  I would like to know if anyone has qualified 1-1/4Cr 1/2Mo to -40 and what special measures were taken to achieve it;  i.e special filler metal requirements or specific filler metal employed, special weld techniques or parameter restrictions, etc.  Materials are SA-387 Grade 11 Class 2 and SA-182 F11 Class 2.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...