[MW:19067] RE: 19048] Mode of Metal transfer for GMAW

Dear Pradip,

   There are 4 modes of metal transfer available for GMAW process.

1.       Short circuit

2.       Globular

3.       Spray( For Argon use)

4.       Pulsed

 

In your case short circuiting mode will be given better result than compare with other modes of transfer, but make sure that your welder skill is playing major role to maintain torch angle etc..

 

Regards,

J.V.S.Hemanth kumar

 

Senior Engineer

Operations I Welspun Middle East Pipes LLC

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pradip Ghosh
Sent: Wednesday, October 23, 2013 7:39 AM
To: materials-welding@googlegroups.com
Subject: [MW:19048] Mode of Metal transfer for GMAW

 

Dear Expert,

 

Can any one tell me that what are the metal transfer mode available for GMAW and what type of metal transfer is suitable for down hand bottom fillet welding in MAG/GMAW

 

 

Pradip Ghosh

 

QA/QC Engineer

 

Mott Mac Donald 

 

 

 

 

 

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Re: [MW:30066] Diameter qualified for set in nozzle

refer IX-80-67 On Mon, 16 Sep 2019 at 12:56, Muhammed Ibrahim PK < ibratech@gmail.com > wrote: Gents,  Is there any interpretation available for set in type nozzle welding diameter not essential variable for welder qualification?. Reg --  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmhNusk1TKk-%3D0t%3Dfcyz0NnpVGvN3Wisj1mL%2B9aoAoRnA%40mail.gmail.com .

Re: [MW:30053] Re: pwps format required

Any body can clarify about  pre heating of ss  pipe joints  in -25°c climet  site work... need pre heating  or no... waiting for your valuable replay On Fri, 13 Sep 2019, 5:39 pm Bien_ND / weldinginspections.net , < bck055@gmail.com > wrote: Hello, get free WPS and PQR format at 1- WPS for SMAW: https://lnkd.in/fevanEM 2- WPS for GTAW: https://lnkd.in/fzYnQKP 3- WPS for GTAW + FCAW: https://lnkd.in/fxMryha 4- WPS for GTAW + SMAW: https://lnkd.in/fQVJFN7 5- WPS for GTAW + SAW: https://lnkd.in/fjW6gvq 6- WPS for GTAW + GMAW: https://lnkd.in/fJ_mzK4 On Wednesday, September 11, 2019 at 3:51:59 PM UTC+7, Dharma dattu wrote: Hello All, we need to establish a wps with SMAW + SAW process, can you share the format. my doubt is will it be called as welder qualification  or (welding operator qualification). Regards, DD -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Go...