Skip to main content

Re: [MW:19132] Re: Crane supporting beam repair

i thinks it is S690 Lincoln  also suggest this and i like this suggestion cause it is the most strongest grade can be so we are in safe side 

Can you send me the specification of this grade?

Regards,
H.A


On Wednesday, October 30, 2013 3:52 PM, Pieper QSI <info@pieper-qsi.nl> wrote:
Depending on the age of the Crane in my opinion it can be S355, S460 or S690 material. That is why I suggest to execute some mechanical tests on the material.
 
Met vriendelijke groeten / Best Regards,
 
Herman Pieper
QA-QC Inspector / IWI-C Welding Inspector / IWT / Materials Expert
 
Logo nieuw klein
Job van der Havestraat 6
8384 DB, Wilhelminaoord
Cell: +31 6 51691215
 
Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens hany alfy
Verzonden: woensdag 30 oktober 2013 10:06
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:19123] Re: Crane supporting beam repair
 
Dear 
 
High tensile steel you mean S355 or you meant another type ?
can you please specify the specification of the said Grade?
 
Regards,
H.A
 
On Tuesday, October 29, 2013 4:39 PM, hpi001 <info@pieper-qsi.nl> wrote:
The beam will be made of a high strength steel in order to reduce the weight. In most of the cases such cracks are being caused by fatigue. It seems to me that the welds present on the first picture have bad transition at weld toe and that undercuts are present at the side of the weld which may initiate fatigue cracks. If you want to repair this beam in my opinion you need to replace a part of the beam flanges in order to distribute the stresses caused by welding activities, and a new stiffener plate need to be put in place. I would suggest to use a high frequency hammering technology, such like Pneumatic Impact Treatment in order to reduce the tensile stresses caused by welding at the surface and to introduce beneficial compressive stresses in order to increase the fatigue strength of the new welds. 
The removed part can be used for mechanical testing in order to determine the actual kind of material. I would suggest a minimum of tensile test and chemical analyses.
 
Best Regards,
 
Herman Pieper

Op maandag 28 oktober 2013 10:28:02 UTC+1 schreef hany alfy:
 
Dear Experts
 
Regarding the A/M Subject please find attached photos for Crane Manitowc support beams 
 
I Need your opinion what will be the grade of this beam and how to repair the cracks in these photos
 
Regards,
H.A
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...