Re: [MW:19047] SET PRESSURE FOR PRESSURE RELIEF VALVE FOR HYDROTESTING OF POWER PIPING

Dear Mr. Dave 

As per our client's requirement, we calibrate the RV at 1.1 times of the actual test pressure.

Regards 

LALU R.P


On Tue, Oct 22, 2013 at 7:45 PM, Ratheesh Ramachandran <pkrratheesh@gmail.com> wrote:
Dear Mr. Srinivasan,

         you can refer to SAES A 004 for relief valve set pressure requirements

regards
Ratheesh.R
Ksa

On Tue, Oct 22, 2013 at 5:50 PM, srini vasan <nevazz21@gmail.com> wrote:
> dear reddy
>
> can i know in what std in aramco mentioned to test the RV 5% Above test
> pressure.
>
> with regards
> N.Srinivasan
>
>
> On Sunday, February 10, 2008 3:08:16 PM UTC+5:30, Sankepalli R.S.Reddy
> wrote:
>>
>> As per aramco project specifications, Test RVs to be set at 5% above test
>> pressure and tested within 1week/1month for new projects/maintenance work,
>> respectively.
>> regards
>>
>>
>> On 1/30/08, shailesh dave <snd...@yahoo.com> wrote:
>>>
>>> Dear Mr Dave
>>> Could you please resend this query with proper subject line? And also in
>>> future please don't hit reply button while starting new thread, instead u
>>> can create new mail and send to
>>> material...@googlegroups.com
>>>
>>> Best regards
>>> Raghuram Bathula
>>> ________________________________
>>> From: shailesh dave [mailto:snd...@yahoo.com]
>>> Sent: Wednesday, January 30, 2008 1:46 PM
>>> To: material...@googlegroups.com
>>> Subject: Re: [MW:537] Re: 533] Filler metal for P 11 (O/L SS 347) to P8
>>>
>>> Dear Members,
>>>
>>> Can anybody tell me at what pressure of hydrotest be safety relief valve
>>> set. What is the reference code.
>>>
>>> Regards,
>>>
>>> S.N.Dave
>>>
>>> QA/QC Manager
>>>
>>>
>>> ________________________________
>>> Never miss a thing. Make Yahoo your homepage.
>>>
>>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...