Re: Fwd: [MW:19121] Change in Supplementary Essential Need re-qualification?

It does not required re qualification.

Regards,

Zakir Ali.


From: Ezat Adel <ezatadel2008@gmail.com>
Sent: Wed, 30 Oct 2013 11:59:27
To: materials-welding <materials-welding@googlegroups.com>
Subject: Fwd: [MW:19118] Change in Supplementary Essential Need re-qualification?
FIRST MY CASE WITHOUT IMPACT TEST REQUIREMENT

IF I HAVE PQR for  P-No. 1 Gr.No.1  to  P-No. 1 Gr.No.1

I CAN USE IT TO WELD  P-No. 1 Gr.No.1  to  P-No. 1 Gr.No.2  ,THAT IS
THE MEANING OF SUPPLEMENTARY ESSENTIAL

EZZAT

---------- Forwarded message ----------
From: george.dilintas@gr.bureauveritas.com
Date: Tue, 29 Oct 2013 11:53:41 +0200
Subject: Re: [MW:19112] Change in Supplementary Essential Need re-qualification?
To: materials-welding@googlegroups.com


It needs

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector
Prelude FLNG ASME Subject Matter Expert

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS

Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Korea cell phone: +82 10 2777 8922



From:   Ezat Adel <ezatadel2008@gmail.com>
To:   materials-welding@googlegroups.com
Date:   29/10/2013 11:25
Subject:   Re: [MW:19109] Change in Supplementary Essential Need
           re-qualification?
Sent by:   materials-welding@googlegroups.com



dear Dr. Georgios Dilintas i need your confirm it is need requalification
or did not need.


On Oct 29, 2013 11:05 AM, <george.dilintas@gr.bureauveritas.com> wrote:


     Yes it does
           best regards

           Dr. Georgios Dilintas

           Authorized Nuclear Inspector
           Authorized Inspector Supervisor
           API 510 Inspector
           Prelude FLNG ASME Subject Matter Expert

           I&F REGIONAL TECHNICAL MANAGER
           BUREAU VERITAS HELLAS

           Tel: +30 210 40 63 113/4
           Fax: +30 210 40 63 118
           Cell: +30 69 44 64 62 04
           Korea cell phone: +82 10 2777 8922



     Inactive hide details for Ezat Adel ---29/10/2013 10:57:21---Dear
     Experts, i need your clarify that the changes in material groEzat
     Adel ---29/10/2013 10:57:21---Dear Experts, i need your clarify that
     the changes in material group number with the

     From: Ezat Adel <ezatadel2008@gmail.com>
     To: materials-welding <materials-welding@googlegroups.com>
     Date: 29/10/2013 10:57
     Subject: [MW:19105] Change in Supplementary Essential Need
     re-qualification?
     Sent by: materials-welding@googlegroups.com



     Dear Experts,

     i need your clarify that the changes in material group number with
     the
     same p number need another welding qualification or not.

     my case i have WPS for A312  grade TP 316, P no. 8 , group no. 1 to
     itself.
     it's right to use it to weld  A312  grade TP 310s, P no. 8 , group
     no.
     2 to itself.

     Ezzat

     --
     To post to this group, send email to
     materials-welding@googlegroups.com
     To unsubscribe from this group, send email to materials-welding
     +unsubscribe@googlegroups.com
     For more options, visit this group's bolg at
     http://materials-welding.blogspot.com/
     http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm


     The views expressed/exchnaged in this group are members personel
     views and meant for educational purposes only, Users must take their
     own decisions w.r.t. applicable code/standard/contract documents.
     ---
     You received this message because you are subscribed to the Google
     Groups "Materials & Welding" group.
     To unsubscribe from this group and stop receiving emails from it,
     send an email to materials-welding+unsubscribe@googlegroups.com.
     For more options, visit https://groups.google.com/groups/opt_out.

     This message contains confidential information. To know more, please
     click on the following link: http://disclaimer.bureauveritas.com


     --
     To post to this group, send email to
     materials-welding@googlegroups.com
     To unsubscribe from this group, send email to materials-welding
     +unsubscribe@googlegroups.com
     For more options, visit this group's bolg at
     http://materials-welding.blogspot.com/
     http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm


     The views expressed/exchnaged in this group are members personel
     views and meant for educational purposes only, Users must take their
     own decisions w.r.t. applicable code/standard/contract documents.
     ---
     You received this message because you are subscribed to the Google
     Groups "Materials & Welding" group.
     To unsubscribe from this group and stop receiving emails from it,
     send an email to materials-welding+unsubscribe@googlegroups.com.
     For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding
+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm


The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an
email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


This message contains confidential information. To know more, please
click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google
Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send
an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments