Skip to main content

Re: [MW:17772] Welding inside CO2 Absorber

Dear Ritolia,

Pl. refer to API 510 to carry out the inspection and welding methods to avoid PWHT of inservice post weld heat treated vessel.

Regards,

PARAG PANSARE

On May 23, 2013 6:09 PM, "B M Ritolia" <bmritolia45@yahoo.com> wrote:
Dear All
We are having Co2 Absorber in our Ammonia plant. This equipment has been installed in 1969. The MOC of vessel is BS 1501-151-28B & is 38mm thick. Now we want to install a new modified demister set on the top of the tower. In this connection demister manufacture wants to weld a
supporting ring (10 MM thk 516 Gr. 70) and 4 nos. brackets (516 Gr. 70). As per supplier, the brackets are to be welded at top conical portion 38 mm thk. (90 Degree orientation) of the absorber. After this 10 mm thk supporting ring is also to be welded to the absorber shell.
As per the drawing of CO2 absorber, the vessel supplier M/S BHPV India have mentioned under the Note;
'NO WELDING IS TO BE DONE ON THE VESSEL AFTER HEAT TREATMENT UNLESS OTHERWISE PERMITTED BY CODE/SPECIFICATIONS".

You are requested to kindly advise regarding welding of 04 nos. brackets and supporting ring (10 MM thk 516 Gr. 70) to absorber shell (38 mm thk. BS-1501-151-28B).kindly also advises welding procedure and type of electrode to be used.

Alternately can we fix the bracket by 8mm dia bolt (4 nos per bracket) after drilling & tapping in the vessel & welding the ring with the bracket? Will it affect the design criteria of the vessel?

Thanks & Regards,

BM Ritolia
Advisor
Kanpur fertilizers & cement ltd.
Udhog Nagar,Panki ,Kanpur
Uttar Pradesh,208022 India

Mob. 07388003288
Land Line 0512-2693504

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...