Short answer is no.  The combination referred to in 200.2 (f) is for a single process with PQRs on performed on multiple thicknesses.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sevak hiren
Sent: Wednesday, November 30, 2011 6:58 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13116] QW-200.4

 

Thanks for explaination, so what does the clause QW-200.1 (f)  mean ? Can't we apply this clause to combine two different processes ?
 


 

On Wed, Nov 30, 2011 at 9:59 AM, manpreet <manpreetsin88@rediffmail.com> wrote:


Hi Aly,

 

Below is interpretation based on Mr. John's wonderful explanation to me in this forum:-

 

Aly's interpretation is correct based on QW-200.4 (b) but if base metal thickness are lesser than 13mm, QW-200.4 (b) does not apply and below would be the answer:-

 

PQR 1- 1.5mm to 12mm

PQR 2- 5mm to 30mm

 

Qualified base metal range: 5mm to 12mm ( 1.5mm < T1 < 12mm, 5mm <

T2 < 30mm )

Maximum Qualified GTAW deposit: 12mm

Maximum qualified SMAW deposit: 12mm

 

QW-200.4 (a) allows you to combine these two PQR’s to support a single WPS. In

such a case the WPS will be restricted to the minimum range qualified by the PQR

base metals (per QW-451); i.e. the intersection of the two individual qualified ranges.

 

QW-200.4(b) is an exception to the general rules for root pass process qualified with a PQR

with base metal thickness > 13mm, and a second PQR for a fill process qualified with a base

metal thickness greater than the base metal thickness used with the root pass PQR.One example of

an acceptable combination would be PQR 1 –13mm thick base metal w/ GTAW root (for the

purpose of example say 6mm deposit thickness, t) combined with PQR 2: 38mm base metal

thickness welded completely by SAW

These conditions would result in a combined WPS such as:

Qualified base metal range: 5mm to 200mm

Qualified maximum GTAW deposit thickness: 12mm

Qualified maximum SAW deposit thickness: 200mm

 

Hope this helps, please let me know if in doubt.

 

Regards

Manpreet Singh




From: "Aly" <mhaskar.aly@gmail.com>
Sent: Tue, 29 Nov 2011 16:10:03
To: <materials-welding@googlegroups.com>
Subject: Re: [MW:13071] QW-200.4

 

Advantage of combining two processes:

 

Suppose u have two wps as below

 

1: WPS with GTAW with 13mm base plate thickness (Base metal Qualification range is 26mm max) 

 

2:WPS with SMAW with 20mm base plate thickness (Base metal Qualification range is 40mm max) 

 

If u combined these two WPS, the advantage you can get is u can weld GTAW process double the max thickness between two process ie  (2 x 20mm = 40mm) not upto 26mm only.

 

You can use more than one WPS in one single joint, just to increase base metal thickness qualification range one can combine two process as per QW-200.4(b).

 

You can create many WPS from one single PQR as needed.

 

Hope this is clear for you..

 

Mhaskar Aly

 

 

 

 

-------Original Message-------

 

From: sevak hiren

Date: 18/11/2011 21:08:13

Subject: [MW:13020] QW-200.4

 

Dear experts....Can anyone provide some Section IX interpretations for clause no.QW-200.4 ?................Can anybody explain this clause better ?...........It clearly states that multiple wps of different processes can be combined together and we can make a single wps combining that processes...........and from one pqr combining different processes ,individual wps can be prepared for each process..............the root deposites clause of min 13 mm is an ALTERNATE requirement....is it really applicable in which situation ?...............

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.




--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please visit http://www.symanteccloud.com
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please visit http://www.symanteccloud.com
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...